Style | Business |
Thickness | 7.5mil, 10mil |
IR Rejection | 0.6 |
UV Rejection | 0.99 |
Material | TPU, Aliphatic TPU |
Position | Body |
Function | Self Healing, Sand Proof, Anti-Scratch, Hydrophobic, Rubble Prevention |
Warranty | More than 5 years |
Color | Transparent Clear |
Usage | Self-adhesive |
Parameter | Test Method | Result |
---|---|---|
Temperature Resistance | -122°F--230℉ | √ |
Thermal Repair Performance | Copper Brush Under 5KG Pressure, 176°F Hot Water | √ (90%+ repair in seconds) |
Chemical Resistance | 10% Sulfuric Acid/Sodium Hydroxide Immersion (72hr) | √ |
Stain Resistance | ASTM E313 9B | √ |
Stone Chip Impact Resistance | SAEJ 400 | √ |
Puncture Resistance | GB/T 10004 | >18N |
Warranty Coverage | Water Spots, Rain Stains, Yellowing, Surface Distortion | √ |
Style | Business |
Thickness | 7.5mil, 10mil |
IR Rejection | 0.6 |
UV Rejection | 0.99 |
Material | TPU, Aliphatic TPU |
Position | Body |
Function | Self Healing, Sand Proof, Anti-Scratch, Hydrophobic, Rubble Prevention |
Warranty | More than 5 years |
Color | Transparent Clear |
Usage | Self-adhesive |
Parameter | Test Method | Result |
---|---|---|
Temperature Resistance | -122°F--230℉ | √ |
Thermal Repair Performance | Copper Brush Under 5KG Pressure, 176°F Hot Water | √ (90%+ repair in seconds) |
Chemical Resistance | 10% Sulfuric Acid/Sodium Hydroxide Immersion (72hr) | √ |
Stain Resistance | ASTM E313 9B | √ |
Stone Chip Impact Resistance | SAEJ 400 | √ |
Puncture Resistance | GB/T 10004 | >18N |
Warranty Coverage | Water Spots, Rain Stains, Yellowing, Surface Distortion | √ |